Exhaust fabrication
|
|
11-10-2004, 09:12 PM
Post: #7
|
|||
|
|||
|
used co2 to weld, only thing is that where steel meets stainless , rust appears so some sort of rust protection is needed.
Disclaimer: Any errors in spelling, tact, or fact are transmission errors. |
|||
|
« Next Oldest | Next Newest »
|
| Messages In This Thread |
|
Exhaust fabrication - Ivan141 - 11-09-2004, 06:07 PM
[] - LevinGT - 11-10-2004 09:12 PM
[] - The Doctor - 11-11-2004, 02:24 AM
|
| Possibly Related Threads... | |||||
| Thread | Author | Replies | Views | Last Post | |
| 4agZe custom fabrication - need pictures | Okami | 5 | 14,464 |
08-08-2011 03:37 AM Last Post: Saber |
|
| rollcage fabrication ? | shanemck | 2 | 4,209 |
10-23-2008 01:39 AM Last Post: JonT |
|